Melamine impregnated paper manufacturers may have many problems with the pre-curing degree in the process of hot pressing production, which must be solved in time.
For the pre-curing caused by the curing agent is too high, it is necessary to reduce the temperature, reduce the pressure, and shorten the hot-pressing cycle to solve the problem, mainly to slow down the speed of the curing reaction and shorten the reaction cycle; If the pre-curing caused by the dipping and drying temperature is too high, it is also necessary to reduce the temperature, increase the pressure, and prolong the time, in order to improve the fluidity of the glue in the molten state. For melamine-impregnated paper with inconsistent pre-curing degrees, the treatment is more complicated, but for products with a high degree of curing in the first stage, the method of lowering the temperature and increasing the time should be adopted.
For the melamine-impregnated paper with too low volatile content, it is not suitable for production under high temperature conditions, and the hot pressing temperature should be appropriately lowered to slow down the reaction speed.
QUICK LINKS
SPANISH FLYING HORSE
Contact Us
China Office Address: No. 10 Xile Street, Leping Town, Sanshui District, Foshan City 528137
India Office Address: Acme Plaza, Andheri Kurla Road, Andheri East, Mumbai - 400 059, Maharashtra, India
Malaysia Office Address:12038, Jalan Cendrawasih 2,Bandar Putra,Kulai,Johor,Malaysia 81000
Bangkok Office Address:82-86 Soi Charoen Nakhon 50, Samre, Thonburi, Bangkok 10600