During the production process of melamine dipped paper, sometimes pleats or paper breaks may occur. What is the reason for this? Let's take a look.
It may be that the brake of the uncoiler is too strong and the position of the guide roller is wrong when the melamine dipped paper is produced, or the pressure roller on the prepreg roller is too close to the prepreg roller. It is also possible that the tension of the paper dipped in the glue tank is too high, or the tension of the paper in the dryer is too high. Then it is caused by the inappropriate volatile content of the paper from the first dryer to the anilox roll. This problem is also caused by the uneven weight of the base paper, wrinkles, cracks or insufficient wet tensile strength of the base paper.
If the melamine dipped paper is pleated or broken, it is mainly caused by these aspects. I hope you can understand this.
QUICK LINKS
CONTACT US
China Head Office Address: No. 10 Xile Street, Leping Town, Sanshui District, Foshan City, Guangdong, China 528137
Tel: +86-757-87385868;+86-757-83601639
E-mail: idecor@ty-decor.com
Fax.: +86-757-87381508
OVERSEAS OFFICES
India Office Address: Shinto Corp., B7 Hind Saurashtra Industrial Estate, MV Road, Marol, Andheri East, Mumbai 400 059, Maharashtra, India
Tel: +91 89289 03398 (Mr. Sandeep Kedia)
Mob.: +91 98210 24528 (Mr. Sandeep Kedia)
Malaysia Office Address: Kulai, Johor, Malaysia
Tel: +60-19-753 0660 (Mr. Ong)
Bangkok Office Address: 82-86 Soi Charoen Nakhon 50, Samre, Thonburi, Bangkok 10600, Thailand
Tel: +66-81-817-9318 (Mr. Vorapong)