Wood grain paper belongs to wood grain melamine paper. It is an environmentally friendly decoration material. When the wood grain paper is filmed, there will be wrinkles. The editor will explain to you the techniques and methods of how to stick wood grain paper to prevent wrinkles. First of all, when choosing wood grain paper (wood grain melamine paper), it is necessary to choose a good quality product. Take imported wood grain paper as an example, its thickness is 0.42mm, its width is 1.22 meters, and its length is 50 meters. The thickness of 0.42mm is also a key factor for wrinkle resistance. If it is too thin, it will damage the surface of the wood grain paper when it is scraped and pressed. In this way, there will be damaged folds, or when the film is applied too quickly, a large number of air bubbles will appear, and wrinkles will also appear when repairing. So try to choose imported quality wood grain paper products. Below is the method of construction;



1. The choice of tools, when filming wood grain paper, try to use a scraper with good flatness. The first recommendation is the wool felt scraper, which has a high flatness and a certain degree of flexibility. When scraping, it will not damage the skin of the wood grain paper.

2. Control of construction strength. Many users have always believed that great power can produce miracles. This is a wrong understanding. We can use wool felt scrapers to press gently and slowly to ensure that each area is compacted. The method of operation is to start from Slowly push one end to the other end, and the other end should not be close to the base layer. Do not paste it all at once on the base layer for scraping, so that air bubbles are easy to appear.

3. Bubble repair, if there are bubbles, you can use a needle on the bubble to puncture and exhaust, and press it flat.

Summary: How to prevent wrinkling of wood-grained paper basically needs to consider several details, such as the leveling of the base layer, the optimization of tools, and the fine film construction. It is difficult to make these films think of bubble folds.